Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 8103-22 High-Performance Dielectric Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8103-22 High-Performance Dielectric Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AboCast 8103-22 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is used in light emitting diodes and where light-fast transparency is needed.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0411 lb/in³
Part A
1.17 g/cc
0.0424 lb/in³
Part B
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.9 MPa
11300 psi
Elongation at Break 4.9 %
4.9 %
Tensile Modulus 2.84 GPa
412 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 108 °C
226 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
Dielectric Constant 3.0

@Frequency 60.0 Hz,
Temperature 23.0 °C
3.0

@Frequency 60.0 Hz,
Temperature 73.4 °F
3.2

@Frequency 60.0 Hz,
Temperature 100 °C
3.2

@Frequency 60.0 Hz,
Temperature 212 °F
4.1

@Frequency 60.0 Hz,
Temperature 150 °C
4.1

@Frequency 60.0 Hz,
Temperature 302 °F
Dissipation Factor 0.0050

@Frequency 60.0 Hz,
Temperature 23.0 °C
0.0050

@Frequency 60.0 Hz,
Temperature 73.4 °F
0.020

@Frequency 60.0 Hz,
Temperature 100 °C
0.020

@Frequency 60.0 Hz,
Temperature 212 °F
0.070

@Frequency 60.0 Hz,
Temperature 150 °C
0.070

@Frequency 60.0 Hz,
Temperature 302 °F
Arc Resistance >= 150 sec
>= 150 sec
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 100 °C
2.00 - 3.00 hour

@Temperature 212 °F
60.0 - 240 min

@Temperature 120 - 160 °C
1.00 - 4.00 hour

@Temperature 248 - 320 °F
optional
Pot Life 30 min

@Temperature 80.0 °C
30 min

@Temperature 176 °F
>= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Descriptive Properties Value Comments
Arc-Track Free (min) > 2000
2.5 KV
Color Clear
Parts by Weight (pbw) 100
Part A
77
Part B
Thermal Shock Resistance Scale 0 (poor) to 10 (excellent)
Users viewing this material also viewed the following: