Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 4241 High Impact Polystyrene
(discontinued **) DescriptionLACQRENE® 14240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | VDE 0303 |
GEHR Plastics PA 6.6 Nylon 6.6, Dry Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total PSI 7240 High Impact Polystyrene 7240 is a very high impact polystyrene for the extrusion industry. This grade has been designed to be diluted with crystal polystyrene (such as LACQRENE® 140, 1340 or 1540) at higher levels than c.. |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
DuPont Teijin Films Melinex® ST505 Polyester Film, 500 Gauge Melinex® ST505 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic.. |
|||
Surface Resistivity per Square | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
DuPont Teijin Films Melinex® ST505 Polyester Film, 700 Gauge Melinex® ST505 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 4801
(discontinued **) LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow p.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 6631 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC93 |
Total Lacqrene® 740 High Impact Polystyrene
(discontinued **) LACQRENE® alpha 740 is a high gloss, high impact grade of polystyrene.ApplicationWhite goods (washing machines, driers), Toys and games, Garden equipment, All applications needing high gloss with g.. |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | VDE 0303 |
GEHR Plastics PVC-U Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |