Category | Polymer , Thermoplastic , Fluoropolymer , PFA |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | Symalit® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.15 g/cc | 2.15 g/cc | ASTM D792 |
Water Absorption | 0.050 % | 0.050 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | 0.050 % | 0.050 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 23 | 23 | ASTM D785 |
Hardness, Rockwell R | 78 | 78 | ASTM D785 |
Hardness, Shore D | 62 | 62 | ASTM D2240 |
Tensile Strength | 20.7 MPa | 3000 psi | ASTM D638 |
Elongation at Break | 500 % | 500 % | ASTM D638 |
Tensile Modulus | 0.689 GPa | 100 ksi | ASTM D638 |
Flexural Strength | 17.2 MPa | 2500 psi | ASTM D790 |
Flexural Modulus | 0.586 GPa | 85.0 ksi | ASTM D790 |
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 0.517 GPa | 75.0 ksi | ASTM D695 |
Shear Strength | 19.3 MPa | 2800 psi | ASTM D732 |
Izod Impact, Notched | 7.79 J/cm | 14.6 ft-lb/in | ASTM D256 Type A |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 135 µm/m-°C @Temperature -40.0 - 149 °C |
75.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Melting Point | 302 °C | 575 °F | Crystalline, Peak; ASTM D3418 |
Maximum Service Temperature, Air | 260 °C | 500 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Flammability, UL94 | V-0 | V-0 | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Dielectric Constant | 2.1 @Frequency 1e+6 Hz |
2.1 @Frequency 1e+6 Hz |
ASTM D150 |
Dielectric Strength | 3.94 kV/mm | 100 kV/in | Short Term; ASTM D149 |
Dissipation Factor | 0.0001 - 0.001 @Frequency 1e+6 Hz |
0.0001 - 0.001 @Frequency 1e+6 Hz |
ASTM D150 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | Yes | Yes | |
Canada AG | No | No | |
FDA | Yes | Yes | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | Yes | Yes |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Acceptable | Acceptable | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
Alkalies, Weak | Limited | Limited | |
Chlorinated Solvents | Limited | Limited | |
Conductive / Static Dissipative | No | No | |
Continuous Sunlight | Limited | Limited | |
Hot Water / Steam | Acceptable | Acceptable | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Acceptable | Acceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Unacceptable | Unacceptable |