Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Nylatron®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 7.0 %
7.0 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Hardness, Rockwell R 115
115
ASTM D785
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 3.31 GPa
480 ksi
ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 3.17 GPa
460 ksi
ASTM D790
Compressive Strength 110 MPa
16000 psi
10% Def.; ASTM D695
Compressive Modulus 2.90 GPa
420 ksi
ASTM D695
Shear Strength 72.4 MPa
10500 psi
ASTM D732
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.20
0.20
Dry vs. Steel; QTM55007
K (wear) Factor 181 x 10<sup>-8</sup> mm³/N-M
90.0 x 10<sup>-10</sup> in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.105 MPa-m/sec
3000 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature -40.0 - 149 °C
40.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.245 W/m-K
1.70 BTU-in/hr-ft²-°F
ASTM F433
Melting Point 260 °C
500 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 104 °C
220 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
ASTM D648
Flammability, UL94 V-2
V-2
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Dielectric Strength 13.8 kV/mm
350 kV/in
Short Term; ASTM D149
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Color Black-Grey
Machinability 1
1-10, 1=Easier to Machine