Polymer Property : Surface Resistivity per Square = 1.00e+13 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet)
Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet)
Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet)
Surface Resistivity per Square 1.00e+13 ohm
1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Symalit® PVDF (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Total Lacqrene® 1235 High Impact Polystyrene  (discontinued **)
LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of ..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Total Lacqrene® 4241 High Impact Polystyrene  (discontinued **)
DescriptionLACQRENE® 14240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet)
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Duratron® PI D7000 PI Unfilled Polyimide (ASTM Product Data Sheet)
Surface Resistivity per Square 1.00e+13 - 1.00e+14 ohm
1.00e+13 - 1.00e+14 ohm
ASTM D257
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
VDE 0303
GEHR Plastics POM-C Acetal
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
VDE 0303
GEHR Plastics PA 6.6 Nylon 6.6, Dry
Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be ..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
VDE 0303
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber
Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical ..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Total PSI 7240 High Impact Polystyrene
7240 is a very high impact polystyrene for the extrusion industry. This grade has been designed to be diluted with crystal polystyrene (such as LACQRENE® 140, 1340 or 1540) at higher levels than c..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Total PSI 8350 High Impact Polystyrene
8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC60093
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced
TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA..
Surface Resistivity per Square 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
DuPont Teijin Films Melinex® ST504 Polyester Film, 500 Gauge
Melinex® ST504 is a crystal clear, high gloss, heat stabilized polyester film. It can be overprinted with a wide range of solvent-based graphic inks and varnishes, silver conductive and dielectric ..
Surface Resistivity per Square 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
DuPont Teijin Films Melinex® ST506 Polyester Film, 700 Gauge
Melinex® ST506 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic..
Surface Resistivity per Square 1.00e+13 ohm
1.00e+13 ohm
Adhesive side; ASTM D257
3M 4318 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Total Lacqrene® 2901 Medium Impact Polystyrene  (discontinued **)
LACQRENE® 2901 is a very easy flowing, medium impact polystyrene for injection molding. The very high flow of this grade allows for the production of thin wall section or long flow path molding on..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC93
Total Lacqrene® 6631 Impact Polystyrene  (discontinued **)
LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application..
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products.
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
ASTM D257
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet)