Category | Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | Ketron® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
Water Absorption | 0.15 % | 0.15 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | 0.50 % | 0.50 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 103 | 103 | ASTM D785 |
Hardness, Rockwell R | 124 | 124 | ASTM D785 |
Hardness, Shore D | 88 | 88 | ASTM D2240 |
Tensile Strength | 51.0 MPa | 7400 psi | ASTM D638 |
Elongation at Break | 1.0 % | 1.0 % | ASTM D638 |
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Compressive Strength | 131 MPa | 19000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 Type A |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 25.2 µm/m-°C @Temperature -40.0 - 149 °C |
14.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Thermal Conductivity | 0.429 W/m-K | 2.98 BTU-in/hr-ft²-°F | ASTM F433 |
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Maximum Service Temperature, Air | 249 °C | 480 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 232 °C | 450 °F | ASTM D648 |
Flammability, UL94 | V-0 | V-0 | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Dielectric Strength | 21.7 kV/mm | 550 kV/in | Short Term; ASTM D149 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Limited | Limited | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
Alkalies, Weak | Acceptable | Acceptable | |
Chlorinated Solvents | Acceptable | Acceptable | |
Conductive / Static Dissipative | No | No | |
Continuous Sunlight | Limited | Limited | |
Hot Water / Steam | Acceptable | Acceptable | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Acceptable | Acceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Acceptable | Acceptable |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Natural | |
Machinability | 7 | 1-10, 1=Easier to Machine |