Category | Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Molded |
Manufacturer | Quadrant Engineering Plastics Products |
Trade Name | Duratron® PAI |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Water Absorption | 0.35 % | 0.35 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | 1.7 % | 1.7 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell E | 80 | 80 | ASTM D785 |
Hardness, Rockwell M | 119 | 119 | ASTM D785 |
Hardness, Shore D | 90 | 90 | ASTM D2240 |
Tensile Strength | 124 MPa | 18000 psi | ASTM D638 |
Elongation at Break | 5.0 % | 5.0 % | ASTM D638 |
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Compressive Strength | 124 MPa | 18000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 2.41 GPa | 350 ksi | ASTM D695 |
Shear Strength | 124 MPa | 18000 psi | ASTM D732 |
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 Type A |
Coefficient of Friction, Dynamic | 0.30 | 0.30 | Dry vs. Steel; QTM55007 |
K (wear) Factor | 1010 x 10-8 mm³/N-M | 500 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Limiting Pressure Velocity | 0.140 MPa-m/sec | 4000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 27.0 µm/m-°C @Temperature -40.0 - 149 °C |
15.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Thermal Conductivity | 0.259 W/m-K | 1.80 BTU-in/hr-ft²-°F | ASTM F433 |
Maximum Service Temperature, Air | 260 °C | 500 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 278 °C | 532 °F | ASTM D648 |
Glass Transition Temp, Tg | 275 °C | 527 °F | ASTM D3418 |
Flammability, UL94 | V-0 | V-0 | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
Dielectric Constant | 4.2 @Frequency 1e+6 Hz |
4.2 @Frequency 1e+6 Hz |
ASTM D150 |
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Short Term; ASTM D149 |
Dissipation Factor | 0.031 @Frequency 1e+6 Hz |
0.031 @Frequency 1e+6 Hz |
ASTM D150 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Limited | Limited | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
Alkalies, Weak | Limited | Limited | |
Chlorinated Solvents | Acceptable | Acceptable | |
Conductive / Static Dissipative | No | No | |
Continuous Sunlight | Limited | Limited | |
Hot Water / Steam | Limited | Limited | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Acceptable | Acceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Acceptable | Acceptable |
Descriptive Properties | Value | Comments |
---|---|---|
Machinability | 6 | 1-10, 1=Easier to Machine |