Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® A ERV3012 (cond.) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A ERV3012 (cond.) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
(Dry)
Water Absorption 6.7 %
6.7 %
initially dry
Moisture Absorption at Equilibrium 1.8 %
1.8 %
initially dry
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
Elongation at Break 7.5 %
7.5 %
Tensile Modulus 4.10 GPa
595 ksi
Charpy Impact Unnotched 8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V