Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 375 V
375 V
Solution A; IEC 60112
Polimeri Europa Edistir N 1840 Polystyrene
General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm..
Comparative Tracking Index 375 V
375 V
Solution A; IEC 60112
Polimeri Europa Edistir R 321P Polystyrene
Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic..
Comparative Tracking Index 375 V
375 V
IEC 112
Qualchem Danamid AFGF-20 Polyamide 66, 20% Glass Fiber
Reinforced with glass fiberInformation provided by Qualchem Zrt.
Comparative Tracking Index 375 V
375 V
IEC 112
Qualchem Danamid AFGF-30 Polyamide 66, 30% Glass Fiber
Reinforced with glass fiberInformation provided by Qualchem Zrt.
Comparative Tracking Index 375 V
375 V
Polimeri Europa EDISTIR N1841 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-12 General purpose polystyrene combining easy flow and medium heat. This grade exhibits excellent processability in ..
Comparative Tracking Index 375 V
375 V
Solution A, Rating; IEC 60112
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
Comparative Tracking Index 375 V
375 V
IEC 60112
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance
Comparative Tracking Index 375 V
375 V
d.a.m.; Solution A; IEC 60112
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Comparative Tracking Index 375 V
375 V
IEC 60112
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose..
Comparative Tracking Index >= 375 V
>= 375 V
IEC 60112
SABIC Innovative Plastics LNP THERMOCOMP PF005 PA 6 (Europe-Africa-Middle East)
25% glass fibre reinforced Polyamide 6 injection moulding resin.
Comparative Tracking Index 375 V
375 V
IEC 60112
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East)
Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Comparative Tracking Index 375 V
375 V
Solution B; IEC 60112
Solvay TECHNYL® A 208F PA66, DRY
Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta..
Comparative Tracking Index 375 V
375 V
IEC 60112
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E..
Comparative Tracking Index 375 V
375 V
IEC 60112
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Comparative Tracking Index 375 V
375 V
Solution A; IEC 60112
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
Comparative Tracking Index 375 V
375 V
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate
Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers, indicator and brake light lenses.Information provided by Bayer.As of 1 September 2015, Ba..
Comparative Tracking Index 375 V
375 V
Covestro Apec® HT KU 1-9333 High-Heat Polycarbonate
Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Comparative Tracking Index 375 V
375 V
IEC 60112
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Comparative Tracking Index 375 V
375 V
M; IEC 60112
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded
BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Comparative Tracking Index 375 V
375 V
M; IEC 60112
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Comparative Tracking Index 375 V
375 V
M; IEC 60112
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Comparative Tracking Index 375 V
375 V
M; IEC 60112
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded
AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Comparative Tracking Index 375 V
375 V
BASF Polystyrol® 165 H Polystyrene (Europe)
High molecular grades, often blended with high-impact extrusion grades (e.g. for dairy products).Data was collected by ISO methods and provided by BASF.
Comparative Tracking Index 375 V
375 V
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe)
Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF.
Comparative Tracking Index 375 V
375 V
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe)
Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF.
Comparative Tracking Index 375 V
375 V
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe)
Very easy-flowing, impact-modified grade.Data was collected by ISO methods and provided by BASF.
Comparative Tracking Index 375 V
375 V
Test solution A; IEC 60112
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Comparative Tracking Index 375 V
375 V
Test solution B; IEC 60112
BASF Ultradur B 6550 L PBT
Ultradur B 6550 L is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes.
Comparative Tracking Index 375 V
375 V
Test Solution A; IEC 60112
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT
Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, ..