Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
Nilit FRIANYL A63 GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
Nilit FRIANYL A63 HH-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
Nilit FRIANYL A63 TF-GV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | IEC 112 |
Qualchem Danamid AFGFS2HUV14 Polyamide 66, 14% Glass Fiber Reinforced with glass fiber. Impact modified, heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial lights.Information provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 550 V | 550 V | IEC 112 |
Qualchem Danamid FGFH-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat stabilized, for long-lasting use at 120-140°C.Information provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 550 V | 550 V | CTI-M 100; IEC 112 |
Nilit FRIANYL A63 K Nylon 6.6 for injection molding Nylon 6.6 for injection molding, formulated for the coloration of button baths.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | |
Radici Radilon® S RCV3015 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Comparative Tracking Index | 550 V | 550 V | A solution |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Comparative Tracking Index | 550 V | 550 V | UL 746 |
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302.. |
|||
Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6 Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr.. |
|||
Comparative Tracking Index | 550 V | 550 V | IEC Method |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6600 GV 5 HWCP 5% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | VDE 0303-P1, IEC 112 |
EPICHEM Epinyl PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre, excellent mechanical properties |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Comparative Tracking Index | 550 V | 550 V | Test Solution A; IEC 60112 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |
Addiplast Addinyl B2 G10 V20 Nylon 6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Comparative Tracking Index | 550 V | 550 V | Test Solution A; IEC 60112 |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Comparative Tracking Index | 550 V | 550 V | Test solution A; IEC 60112 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
DSM Akulon® K220-HGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(discontinue The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 550 V | 550 V | |
Radici Radilon® A RV350 (cond) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Comparative Tracking Index | 550 V | 550 V | UL 746 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Comparative Tracking Index | 550 V | 550 V | Conditioned; UL 746 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |
Addiplast Addinyl B2 V30 Nylon 6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |