Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 450 V | 450 V | STN EN 60112 |
Plastcom PLASTAMID® 66 GF 15 T 15 TS PA66 reinforced with glass fibers and mineral filler, heat stabilized Black PA66 for injection molding, reinforced with 15% glass fiber and 15% mineral filler, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of elect.. |
|||
Comparative Tracking Index | 450 V | 450 V | STN 34 6468 |
Plastcom SLOVAMID 66 GF 10 GB 20 Polyamide 66, 10% Glass Fiber, 20% Glass Beads FeaturesPA 66 chemically reinforced with 10% glass fiber and with the content of 20% glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can .. |
|||
Comparative Tracking Index | 450 V | 450 V | STN 34 6468 |
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Comparative Tracking Index | 450 V | 450 V | UL746A |
Shell Carilon® DB6F1G30 Polyketone, Flame-Retarded, Tracking-Resistant, Glass-Reinforced Injection Molding Grade
&n Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F1G30 is a flame-retarded, 15 percent glass-fiber-reinforced, injection molding grade with mecha.. |
|||
Comparative Tracking Index | 450 V | 450 V | |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |
|||
Comparative Tracking Index | 450 V | 450 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 H-SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 450 V | 450 V | |
Ineos ABS NOVODUR® L3FR ABS, Injection Grade
(discontinued **) Injection molding grade, flame retardant, very easy flow. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Television and computer housings.Information provided by the manufact.. |
|||
Comparative Tracking Index | 450 V | 450 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, DRY Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
Comparative Tracking Index | 450 V | 450 V | IEC 60112 |
SABIC Innovative Plastics NORYL V081 PPE+HIPS (Europe-Africa-Middle East) NORYL V081 is a high flow, UV stabilized PPO/PS blend for TV backplate applications. |
|||
Comparative Tracking Index | 450 V | 450 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Comparative Tracking Index | 450 V | 450 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Comparative Tracking Index | 450 V | 450 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Comparative Tracking Index | 450 V | 450 V | IEC 112 |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Comparative Tracking Index | 450 V | 450 V | IEC 112 |
Supreme Petrochem SP 556 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect.. |
|||
Comparative Tracking Index | 450 V | 450 V | Solution B; IEC 60112 |
Solvay TECHNYL® 27010ST PA66, DRY Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of.. |
|||
Comparative Tracking Index | >= 450 V | >= 450 V | KA Method; IEC 112; DIN 53480 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWCP 50% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6600 MR 209 HWCP 20% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6600 MZ 315 CP Combination Nylon 66, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | >= 450 V | >= 450 V | IEC 1212-2 6.4 |
Hippe SI GC 202 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in mechanical and electrical applications at elevated temperature. Good heat resistance.Information provided by Hippe. |
|||
Comparative Tracking Index | 450 V | 450 V | M; IEC 60112 |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Comparative Tracking Index | 450 V | 450 V | Test solution A; IEC 60112 |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Comparative Tracking Index | 450 V | 450 V | Test solution A; IEC 60112 |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Comparative Tracking Index | 450 V | 450 V | Test solution A; IEC 60112 |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
Comparative Tracking Index | 450 V | 450 V | Test Solution A; IEC 60112 |
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned) Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade. |
|||
Comparative Tracking Index | 450 V | 450 V | Test Solution A; IEC 60112 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000 GS 25 HWCP 25% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |