Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 300 V | 300 V | |
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Covestro Bayblend® KU 2-1473 Polycarbonate/ABS Blend
(discontinued **) Matter surfaces than standard grades; injection molding.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new nam.. |
|||
Comparative Tracking Index | 300 V | 300 V | Test liquid A; IEC 60112 |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Comparative Tracking Index | 300 - 450 V | 300 - 450 V | Average value: 390 V Grade Count:5 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Comparative Tracking Index | 300 V | 300 V | Solution B; IEC 60112 |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
Teijin Panlite® LS-2250 Friction and Abrasion Resistant Polycarbonate Resin It is compounded with fluorine powder to improve friction and abrasion resistance, meeting UL 94 V-2. The friction and abrasion resistance is superior than that of polyamidoacetal, maintaining excel.. |
|||
Comparative Tracking Index | 300 V | 300 V | UL 746 |
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Comparative Tracking Index | 300 V | 300 V | IEC Method |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and very good hydrolysis resistance antimony-, chlorine- and bromine-free flame.. |
|||
Comparative Tracking Index | 300 V | 300 V | Solution A; IEC 60112 |
Covestro Bayblend® FR3050 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Comparative Tracking Index | 300 V | 300 V | Solution A; IEC 60112 |
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
DSM Stanyl® TW200F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Comparative Tracking Index | 300 V | 300 V | |
BASF Luranyl® KR 2404 Polyphenylene Ether + Styrene-Butadiene Blend Base grade with high heat deformation resistance and a balanced combination of stiffness and toughness. Uses include: steering-wheel covers and heater controls.Data was collected by ISO methods and.. |
|||
Comparative Tracking Index | >= 300 V | >= 300 V | 2824-1975 |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Comparative Tracking Index | 300 V @Temperature 23.0 °C |
300 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Comparative Tracking Index | >= 300 V | >= 300 V | Solution A; Ø 93x3mm; IEC 112 |
SYNTHOS Krasten® 336M High Impact Polystyrene Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos. |
|||
Comparative Tracking Index | >= 300 V | >= 300 V | Solution A; Ø 93x3mm; IEC 112 |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 112 |
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Polimeri Europa KOBLEND PCA 53 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 110°C Main application fiel.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Polimeri Europa KOBLEND PCA 628 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Extrusion grade with very good toughness. Main application fields: automotive small profilesUnfilled. Suitable for Extrusion, Thermoforming. Supplied as pe.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Polimeri Europa KOBLEND PCA 638 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with very good impact behaviour even at low temperatures, good dimensional stability. Vicat/B50 = 120°C Main application fields: au.. |
|||
Comparative Tracking Index | 300 V | 300 V | Test solution A; IEC 112 |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
Lanxess Pocan® A 3131 000000 PBT+ASA, 30% glass fibers PBT+ASA, 30% glass fibers, injection molding, low tendency to warp, improved surface finish |