Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 1.00e+11 ohm | <= 1.00e+11 ohm | ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for .. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free
(discontinued **) Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Surface Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
95% RH, 48 hrs |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
Surface Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
95% RH, 48 hrs |
Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elev.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, Conditioned Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® C 246 M PA6, DRY Description: Unreinforced polyamide 6, with high impact resistance, for injection molding. Grade formerly known as PSB196.Available in: EuropeProduct Applications: It is particularly adapted to the .. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF55 HS L OR016 57% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 57% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Asia Pacific) LNP* Stat-loy* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® TR XE 4010 PA*-I Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fat.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® TSM-40/4 PA666-MD40 Product description: Grilon TSM-40/4 is a special heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 40% mineral filler. Grilon TSM-40/4 has the following important properties.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® TSS/2 FA PA666 Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow .. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 3959 nat PA610 Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materia.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 4071 nat PA612-I Product description: Grilamid XE 4071 NATURAL is an unreinforced impact modified high viscosity polyamide 612 (PA612) extrusion grade with superior hydrolysis and heat resistance. Compared to standa.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40 Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30 Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Adamas Adalon® 509 PTFE, 3% MoS2 Information provided by Adamas, HPM |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | CEI 60093 |
Addiplast Addilene H 555 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | CEI 60093 |
Addiplast Addilene PMD 50258 Polypropylene Copolymer For electroplatingInformation provided by Addiplast. |
|||
Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | DIN 53482/VDE 0303 |
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Adamas Adalon® 508 PTFE, 1% MoS2 Information provided by Adamas, HPM |
|||
Surface Resistance | 1.00e+11 - 3.16e+11 ohm | 1.00e+11 - 3.16e+11 ohm | IS 3396-1979 |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Adamas Adalon® 510 PTFE, 5% MoS2 Information provided by Adamas, HPM |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |