Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Water Absorption 0.55 %

@Time 86400 sec
0.55 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 183 MPa
26500 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.4 µm/m-°C
18.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 259 °C
499 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
ASTM D257
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
ASTM D257
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149