Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elevated temperatures.Comments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI UnitsData provided by Chevron Phillips Chemical Company LP.Solvay Specialty Polymers has acquired the Ryton product line.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 150 MPa
21800 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
Flexural Yield Strength 185 MPa
26800 psi
ASTM D790
Flexural Modulus 15.0 GPa
2180 ksi
ASTM D790
Compressive Yield Strength 240 MPa
34800 psi
ASTM D695
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 21.0 µm/m-°C

@Temperature 100 - 200 °C
11.7 µin/in-°F

@Temperature 212 - 392 °F
Axial; ASTM E831
21.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
11.7 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ASTM E831
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
84.0 µm/m-°C

@Temperature 100 - 200 °C
46.7 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.320 W/m-K
2.22 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
UL Temperature Index 200 / 220 per UL746B
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Annealed 2 hr @ 200°C; ASTM D659
Flammability, UL94 5VA
5VA
UL94 V-0/5VA
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Surface Resistance 1.00e+11 ohm

@Temperature 90.0 °C
1.00e+11 ohm

@Temperature 194 °F
95% RH, 48 hrs
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
ASTM D150
3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
457 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
0.0020

@Frequency 1e+6 Hz
0.0020

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 sec
125 sec
ASTM D495
Comparative Tracking Index 130 V
130 V
UL 746A
Users viewing this material also viewed the following: