Polymer Property : Surface Resistance = 10 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX AS003 ABS
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX KX88084 POM (Europe-Africa-Middle East)
LNP* Faradex* KX88084 is a compound based on POM resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Surface Resistance 10 - 100 ohm
10 - 100 ohm
ASTM D257
PolyOne Therma-Tech™ NJC-6000 TC Nylon 12  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Surface Resistance <= 10 ohm
<= 10 ohm
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Surface Resistance 10 ohm
10 ohm
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; ..
Surface Resistance 10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI
LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Surface Resistance 10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI (Asia Pacific)
LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated.
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D257
SABIC Innovative Plastics LNP LUBRICOMP JX00061 PES (Europe-Africa-Middle East)
LNP* Lubricomp* JX00061 is a compound based on Polyethersulfone resin containing Carbon Fiber, Proprietary Lubricant. Added features of this material include: Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP LUBRICOMP RCL36XXP PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RCL36XXP is a compound based on PA 66 resin, containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS (Asia Pacific)
LNP* Stat-kon* AX02747 is a compound based on Acrylonitrile Butadiene Styrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
Techmer ES Electrablend® PPS 05002
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc.
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE006 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE006 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC
LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan..
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon DEL369E PC
LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S..
Surface Resistance 10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DSL229 PC
LNP* STAT-KON* DSL229 is a compound based on Polycarbonate resin containing 10% PTFE, 10% Stainless Steel. Added features of this material include: Electrically Conductive, Wear Resistant.
Surface Resistance 10 - 100 ohm
10 - 100 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON OE008A PPS - Branched (Europe-Africa-Middle East)
LNP* Stat-kon* OC-1008 is a compound based on PPS - Branched resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Surface Resistance 10 - 100 ohm
10 - 100 ohm
ASTM D257
Techmer ES Luriblend® PS 06001
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler/Unspecified FillerReinfor.Information provided by TP Composites, Inc.
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East)
LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
IEC 60093
Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin
CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica..
Surface Resistance 10 ohm - 1e+05
10 ohm - 1e+05
ASTM D257
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer (Asia Pacific)
LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing Carbon Fiber. Added features of this material include: Clean Compounding System.
Surface Resistance 10 - 100 ohm
10 - 100 ohm
ASTM D257
SABIC Innovative Plastics LNP THERMOCOMP RC008ESS PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RC008ESS is a compound based on PA66 resin containing Carbon Fiber. Added features include; Electrically Conductive, Easy Molding, Heat Stabilized.
Surface Resistance 10 - 100 ohm
10 - 100 ohm
ASTM D257
SABIC Innovative Plastics LNP THERMOCOMP RC00A PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RC00A is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON KX97157 Acetal Copolymer (Europe-Africa-Middle East)
LNP* STATKON* KX97157 is a compound based on Acetal resin containing Carbon. Added features include : Electrically Conductive, Impact Modified.