Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 2.50 mm |
15 - 30 sec @Thickness 0.0984 in |
PLC 3 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.50 mm |
15 - 30 sec @Thickness >=0.0984 in |
|
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.50 mm |
15 - 30 sec @Thickness >=0.0984 in |
|
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical LUPOL GP1007F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.30 mm |
15 - 30 sec @Thickness >=0.130 in |
|
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 0.749 mm |
15 - 30 sec @Thickness 0.0295 in |
UL 746 |
Teknor Apex APEX® 94-A0055A-80 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 94-A0055A-80 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |