Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex APEX® 94-A0055A-80 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 94-A0055A-80 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: 60°C General Purpose; RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
15 seconds; ASTM D2240
Tensile Strength at Break 15.9 MPa
2300 psi
ASTM D638
Elongation at Break 390 %
390 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Flammability, UL94 HB

@Thickness 0.749 mm
HB

@Thickness 0.0295 in
ALL
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
ALL
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
ALL
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V

@Thickness 3.00 mm
>= 600 V

@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 0.749 mm
15 - 30 sec

@Thickness 0.0295 in
UL 746
15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
UL 746
15 - 30 sec

@Thickness 3.00 mm
15 - 30 sec

@Thickness 0.118 in
UL 746
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: