Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 220 °C | 428 °F | |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 220 °C | 428 °F | |
Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, Medium Slip, Medium Antiblock Version of 7109TCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-301 Flame Retardant Polystyrene Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa H-12 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT HB9255D Ester Type TPE Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
LG Chemical LUCON PS4200 ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | Injection Molding |
Styrolution Luran® 378 P G7 35% Glass Filled SAN Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Borealis HE125MO Polypropylene HE125MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by good flow properties and high stiffness in and is specially suitable for high-speed injection mo.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Borealis HH450MO Polypropylene HH450MO is a polypropylene homopolymer intended for injection molding. This grade is especially suitable for high-speed injection molding of articles demanding easy flow. This polymer is a CR (cont.. |
|||
Melt Temperature | 220 °C | 428 °F | |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Tisan TISLAMID® 6 UNR Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melt Temperature | <= 220 °C | <= 428 °F | |
Total PS CPDS 827 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 827 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 827 can be supplied in both natural and colored forms.Main Characteristics:DBD.. |
|||
Melt Temperature | 220 °C | 428 °F | |
E-Polymers SEPAZ® N3040ST Nanoclay 4% Super Toughness Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
Polyplastic Armlen® PP 3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |
|||
Melt Temperature | <= 220 °C | <= 428 °F | |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |
|||
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
NOVA Chemicals Sclair® 11N1 PE Film Resin
(discontinued **) Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
Sax Polymers SAXALEN PPH325GK20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH325GK20 is a 10% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. It has a increased stiffness and a optimized warpage grade.Information .. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |