Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | Injection |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Melt Temperature | 321 - 338 °C | 610 - 640 °F | Injection |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
&nbs AMODEL AFA-6133 V0 is a 33% glass-fiber reinforced grade of polyphthalamide (PPA) resin that was developed specifically for connector applications requiring compatibility with both "infrared" and "v.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | Injection |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Melt Temperature | 321 - 349 °C | 610 - 660 °F | |
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L 9530 PPS, 55% Mineral
(discontinued **) Good-flow Embedding Compound, Isotropic Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Embedding of Microchips and Electronic ComponentsProcessing: Inject.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber
(discontinued **) High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Clutch Components, BushingsProcessing: Inje.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient.. |
|||
Melt Temperature | 321 - 335 °C | 610 - 635 °F | |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Melt Temperature | 321 - 338 °C | 610 - 640 °F | |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Melt Temperature | 321 - 335 °C | 610 - 635 °F | |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Melt Temperature | 321 - 345 °C | 610 - 653 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; .. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L 9510-1 PPS, 40% Glass Fiber High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Impellers, Valve Housings and BushingsProcessing: Injection Molding (.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L 9560 PPS, 50% Mineral High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1945 HSL Polyphthalamide (PPA)
(discontinued **) Amodel A-1945 HSL is a 45% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers. |