Albis Plastics Tedur® L 9530 PPS, 55% Mineral  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L 9530 PPS, 55% Mineral  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Good-flow Embedding Compound, Isotropic Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Embedding of Microchips and Electronic ComponentsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.92 g/cc
0.0694 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Flexural Yield Strength 100 MPa
14500 psi
DIN 53 452
Flexural Modulus 9.50 GPa
1380 ksi
DIN 53 457
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F