Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE ZS2606 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Melt Temperature | 180 - 240 °C | 356 - 464 °F | Recommended |
NOVA Chemicals Novapol® HE-W959-A HDPE Extrusion/Blow Molding Resin HE-W959-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Lotte Chemical Titan TITANEX® LF1051 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1051 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstandin.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 180 - 280 °C | 356 - 536 °F | Molding |
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic.. |
|||
Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
LATI Latene® EP 7-V2 PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
LATI Latiohm 73/23-10 CNT POM Semiconductive/dissipative product based on Polyoxymethylene (POM). Carbon nanotubes.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Melt Temperature | 180 - 230 °C | 356 - 446 °F | Injection Molding |
Stellarchem AB845EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 180 - 260 °C | 356 - 500 °F | ISO 294 |
Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
Melt Temperature | 180 - 250 °C | 356 - 482 °F | Injection Molding |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Melt Temperature | 180 - 280 °C | 356 - 536 °F | Injection Molding |
Styrolution Polystyrol 165 H GR 21 PS Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo.. |
|||
Melt Temperature | 180 - 260 °C | 356 - 500 °F | |
Supreme Petrochem SC 208 General Purpose Polystyrene CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a .. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Eurostar Star L POM D84 POM, Injection Molded Star L POM D84 is a PTFE/Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 180 - 225 °C | 356 - 437 °F | |
NOVA Chemicals Novapol® LE-0820-AM LDPE Concentrate Resin
(discontinued **) Features: easy processing, good dispersion.Applications: Additive and color concentrates for film and molding, non-critical extrusion coating.Data provided by the manufacturer. |