Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution PS 476L HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Styrolution
Trade Name PS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution PS 476L HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal flow HIPSGood mechanical and heat resistance propertiesEasy processability with short cycle timeInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %

@Temperature 23.0 °C
<= 0.10 %

@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %

@Temperature 23.0 °C
<= 0.10 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ISO 294-4
Melt Flow 5.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO 2039-1
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Elongation at Yield 1.5 %
1.5 %
ISO 527
Tensile Modulus 1.85 GPa
268 ksi
ISO 527
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Flexural Modulus 1.95 GPa
283 ksi
ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
ISO 180/A
Charpy Impact Unnotched 13.0 J/cm²

@Temperature -30.0 °C
61.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75
Vicat Softening Point 90.0 °C

@Load 5.10 kg
194 °F

@Load 11.2 lb
50°C/h; ISO 306
98.0 °C

@Load 1.02 kg
208 °F

@Load 2.25 lb
50°C/h; ISO 306
Optical Properties Metric English Comments
Gloss 35 %
35 %
Specular Gloss, 60°; ASTM D 523
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+18 ohm-cm
>= 1.00e+18 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 60093
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
IEC 60250
Dielectric Strength 155 kV/mm

@Thickness 1.50 mm
3940 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Dissipation Factor 0.00040

@Frequency 1.00e+6 Hz
0.00040

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
ISO 294
Mold Temperature 10.0 - 60.0 °C
50.0 - 140 °F
ISO 294
Injection Velocity 200 mm/sec
7.87 in/sec
ISO 294