Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic  (Unv

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic  (Unv.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intrinsic properties (moldability, low cost, lightness, high mechanical properties), low friction coefficient and low wear are required.Specific Notes for this Material: polyoxymethylene base (POM); 1% molybdenum disulfide; good wear resistance.Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.All data provided by LATI.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Water Absorption 0.15 %
0.15 %
at 23°C; ISO 62
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
LATI
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
LATI
Mechanical Properties Metric English Comments
Hardness, Rockwell M 84
84
ASTM D785
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ISO 527
19.0 MPa

@Temperature 120 °C
2760 psi

@Temperature 248 °F
ISO 527
29.0 MPa

@Temperature 90.0 °C
4210 psi

@Temperature 194 °F
ISO 527
41.0 MPa

@Temperature 60.0 °C
5950 psi

@Temperature 140 °F
ISO 527
Flexural Modulus 2.94 GPa
426 ksi
ASTM D790
0.600 GPa

@Temperature 120 °C
87.0 ksi

@Temperature 248 °F
ASTM D790
0.980 GPa

@Temperature 90.0 °C
142 ksi

@Temperature 194 °F
ASTM D790
1.70 GPa

@Temperature 60.0 °C
247 ksi

@Temperature 140 °F
ASTM D790
Izod Impact, Notched 0.700 J/cm

@Temperature -40.0 °C
1.31 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.700 J/cm

@Temperature -20.0 °C
1.31 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.800 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
ASTM D648
Vicat Softening Point 152 °C
306 °F
50°C/h 50N; ISO 306
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 18 %
18 %
ISO 4589
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
IEC 112
Processing Properties Metric English Comments
Melt Temperature 180 - 200 °C
356 - 392 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 - 100 °C
176 - 212 °F
Temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour
>= 3 hour
Drying time can be reduced when using vacuum ovens.
Descriptive Properties Value Comments
Heat Resistance - Ball Test (125°C) Y
IEC 335
Heat Resistance - Ball Test (165°C) N
IEC 335
Injection Speed medium
Needle Burner Test N
1.47 mm
N
3.05 mm