NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 820 %
820 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 7.80 J/cm
14.6 ft-lb/in
Notched/Unnotched not specified; ASTM D256
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F