Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | |
Premix Thermoplastics PRE-ELEC® ESD 4300 PRE-ELEC ESD 4300 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 4300 has been developed for mult.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Melt Temperature | 170 - 282 °C | 338 - 540 °F | Average value: 219 °C Grade Count:44 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI LASTIROL R-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforc.. |
|||
Melt Temperature | 170 - 220 °C | 338 - 428 °F | |
Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin
(discontinued **) LI5011 is a pelleted high flow linear low density polyethylene. The higher melting point of the resin allows for higher end-use temperatures.Applications: House-wares, toys, lids, containers.Advan.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2607 HDPE Injection Molding Resin Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | Recommended |
NOVA Chemicals Sclair® 72A Butene Copolymer LLDPE Injection Molding Resin 72A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 72A is su.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8306 UV8D, 8306G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 315 °C | 338 - 599 °F | Average value: 231 °C Grade Count:7 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Melt Temperature | 170 - 210 °C | 338 - 410 °F | Start Point: 190°C |
Kingfa FRABS-518 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmLow temperature impact resistanceApplications:Injection moldingPower tools accessoriesInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 °C | 338 °F | |
Lubrizol Estane® ALR G500 Water Absorbent Thermoplastic Polyurethane Type: Estane® ALR G500 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provide.. |
|||
Melt Temperature | 170 - 200 °C | 338 - 392 °F | |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 170 - 210 °C | 338 - 410 °F | |
E-Polymers TEKAFIN® PH70G1 HIPP + 10% Glass Fiber Reinforced Scratch Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8306 BK, 8306G BK MDPE Rotational Molding Resin
(discontinued **) Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 220 °C | 338 - 428 °F | Average value: 200 °C Grade Count:14 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 215 °C Grade Count:51 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 224 °C Grade Count:92 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 205 °C Grade Count:6 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |