| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr.. |
|||
| Melt Temperature | 160 - 190 °C | 320 - 374 °F | |
| NOVA Chemicals Novapol® LF-0219-A LDPE Blow Molding Resin Good heat sealing latitude, Easy processabilityApplications: Food contact, Squeeze bottles, Non-ESCRAdditives: Base resinInformation provided by NOVA Chemicals. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| LATI LASTIROL R-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforc.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| LATI LASTIROL TR-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia.. |
|||
| Melt Temperature | 175 - 190 °C | 347 - 374 °F | |
| Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
| Melt Temperature | 180 - 190 °C | 356 - 374 °F | |
| Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
| Melt Temperature | 160 - 190 °C | 320 - 374 °F | |
| Borealis LE1169 Polyethylene LE1169 is a low loss LDPE compound for coaxial cables. LE1169 contains a special type of antioxidant, which does not adversely affect the electrical properties. Applications: coaxial cables Specifi.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 150 - 190 °C | 302 - 374 °F | Blown Film Coextrusion |
| DuPont™ Appeel® 20D828 Ethylene Acrylate Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp.. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
| Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
| Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Melt Temperature | 140 - 190 °C | 284 - 374 °F | |
| Polyplastic TechnoTep A® 65 A Thermoplastic Elastomer, Mineral Filled Low mineral filled, good flexibilityInformation provided by PolyPlastic Group. |
|||