Material Notes:
PRE-ELEC ESD 4300 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 4300 has been developed for multilayer film blowing. It can also be blow molded or injection molded. Surface resistance values of 109 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters.Typical applications include multilayer bags, sacks and bottles which give permanent ESD protection for the electronics, medical, pharmaceutical and agricultural industries. When PRE-ELEC ESD 4300 is used in the core layer and FDA approved polyolefin in the outer layers, a low charging and food approved film can be achieved. PRE-ELEC ESD 4300 gives also good printability without treatment as it has low surface tension and can be colored into various bright colors.PRE-ELEC ESD 2300 is recommended to be used only in multilayer constructions. Therefore the mechanical properties are dependent on the other layer material.Test Specimen: Monolayer Film.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Electrical Properties Metric English Comments
Surface Resistance 1.00e+9 ohm
1.00e+9 ohm
ISO IEC 61340-5-1
Static Decay <= 2.0 sec
<= 2.0 sec
ISO IEC 61340-5-1
Processing Properties Metric English Comments
Melt Temperature 170 - 195 °C
338 - 383 °F
Blow-up Ratio (BUR) >= 1.8
>= 1.8
Drying Temperature 60.0 °C

@Time 10800 sec
140 °F

@Time 3.00 hour
Pre-drying
Descriptive Properties Value Comments
Screen Pack Standard