Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical KEYFLEX TO1065A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol) Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG .. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID SG4389B PA66+GF/MF38% Feature: Injection Molding, PA66+GF/MF38%Application: Automotive (Fan & Shroud)CAS No. 32131-17-2, 25038-54-4, 65997-17-3 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL EI5002 PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 9002-88-4Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP2150 PP+GF15% Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical SG175 ABS, Super Surface Gloss Feature: Injection Molding, Super Surface GlossApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical XR474 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP3400 PP+MF40% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HM2300 PP+GF30% Description: Injection Molding, PP+GF30%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HR2100D PP+GF17% Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL TE5007B PP+Rubber, High Impact Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP3102 PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |