Polymer Property : Drying Temperature = 219 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 104 - 110 °C
219 - 230 °F
Average value: 107 °C Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Drying Temperature 104 - 110 °C
219 - 230 °F
PolyOne Edgetek® MP-10GF/000 Modified PPO - 10% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Drying Temperature 104 °C
219 °F
Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 78AT0 NAT021 is a soft, polyether based, NHFR thermoplastic polyurethane (TPU) compound.Features: Soft, transparent, flame retardant.Uses: Wire and CableAvailable in Europe, Middl..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane
Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane
Features: Non-Halogenated flame retardant compoundUses: Extrusion – wire and cable and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Afr..
Drying Temperature 104 °C
219 °F
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane
Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane
Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by ..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane
Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi..
Drying Temperature 104 °C
219 °F
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
Drying Temperature 104 °C
219 °F
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
Drying Temperature 104 °C
219 °F
Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane
Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact..
Drying Temperature 104 °C
219 °F
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic
Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol
Drying Temperature 104 °C
219 °F
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Drying Temperature 104 °C
219 °F
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane
Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E..
Drying Temperature 104 °C

@Time 7200 sec
219 °F

@Time 2.00 hour
Lubrizol Estane® 58144 Thermoplastic Polyurethane
Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: ..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane
Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat..
Drying Temperature 104 °C
219 °F
Lubrizol Estane® 58437 Thermoplastic Polyurethane
Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi..
Drying Temperature 104 - 121 °C
219 - 250 °F
Average value: 115 °C Grade Count:7
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane
Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid..