Material Notes:
Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore D 47 - 53

@Time 5.00 sec
47 - 53

@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 64.1 MPa
9300 psi
ASTM D412
Elongation at Break 420 %
420 %
ASTM D412
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
300% Modulus 0.0307 GPa
4.45 ksi
ASTM D412
Tear Strength 31.6 kN/m
180 pli
Trouser; ASTM D470
Graves Tear Strength 140 kN/m
800 pli
Die C; ASTM D624
Tensile Set 12 %
12 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Kofler
170 °C
338 °F
DSC
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
DSC
Processing Properties Metric English Comments
Zone 1 199 °C
390 °F
Extrusion
Zone 2 204 °C
399 °F
Extrusion
Zone 3 210 °C
410 °F
Extrusion
Zone 4 216 °C
421 °F
Extrusion
Adapter Temperature 221 °C
430 °F
5, Extrusion
Die Temperature 221 °C
430 °F
6, Zone 1, Extrusion
221 °C
430 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F