Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Loss On Ignition 32 %
32 %
ASTM D2863
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 93

@Time 5.00 sec
87 - 93

@Time 0.00139 hour
ASTM D2240
Tensile Strength 27.9 MPa
4050 psi
ASTM D412
Elongation at Break 340 %
340 %
ASTM D412/D638
100% Modulus 0.00860 GPa
1.25 ksi
ASTM D412
300% Modulus 0.0148 GPa
2.15 ksi
ASTM D412
Tear Strength 21.9 kN/m
125 pli
ASTM D470
Graves Tear Strength 84.1 kN/m
480 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 2.0
2.0
H18, 1000g; ASTM D3389 B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -38.0 °C
-36.4 °F
DSC
Flammability Test 5.0
5.0
Processing Properties Metric English Comments
Zone 1 183 °C
361 °F
Extrusion
Zone 2 188 °C
370 °F
Extrusion
Zone 3 196 °C
385 °F
Extrusion
Zone 4 199 °C
390 °F
Extrusion
Adapter Temperature 202 °C
396 °F
5, Extrusion
Die Temperature 196 °C
385 °F
Zone 2, Extrusion
202 °C
396 °F
Zone 1, 6, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F