Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type: Estane® ZHF 78AT0 NAT021 is a soft, polyether based, NHFR thermoplastic polyurethane (TPU) compound.Features: Soft, transparent, flame retardant.Uses: Wire and CableAvailable in Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ISO 2781
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 78

@Time 3.00 sec
78

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 30.1 MPa
4370 psi
ISO 527
Elongation at Break 670 %
670 %
ISO 527
50% Modulus 0.00350 GPa
0.508 ksi
100% Modulus 0.00450 GPa
0.653 ksi
300% Modulus 0.00750 GPa
1.09 ksi
Tear Strength 85.2 kN/m
486 pli
Without Nick; ISO 34-1B
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Zone 1 160 °C
320 °F
Zone 2 175 °C
347 °F
Zone 3 180 °C
356 °F
Zone 4 190 °C
374 °F
Adapter Temperature 185 °C
365 °F
Die Temperature 175 °C
347 °F
tip
180 °C
356 °F
180 °C
356 °F
Drying Temperature 104 °C
219 °F
Dry Time 3.00 hour
3.00 hour
Dew Point -40.0 °C
-40.0 °F
Users viewing this material also viewed the following: