| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade |
| Manufacturer | Lubrizol (former Noveon) |
| Trade Name | ESTANE® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | flex bar, Injection |
| 0.0090 cm/cm | 0.0090 in/in | disk, Injection |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 62 - 68 @Time 5.00 sec |
62 - 68 @Time 0.00139 hour |
ASTM D2240 |
| Tensile Strength | 41.0 MPa | 5950 psi | ASTM D412 |
| Elongation at Break | 430 % | 430 % | ASTM D412 |
| 100% Modulus | 0.0210 GPa | 3.05 ksi | ASTM D412 |
| 300% Modulus | 0.0310 GPa | 4.50 ksi | ASTM D412 |
| Flexural Modulus | 0.372 GPa | 54.0 ksi | ASTM D790 |
| Tear Strength | 50.8 kN/m | 290 pli | ADM D470 |
| Graves Tear Strength | 210 kN/m | 1200 pli | Die C; ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 19 | 19 | CS-17, 1000g; ASTM D3389 B |
| Compression Set | 42 % @Temperature 23.0 °C, Time 79200 sec |
42 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| 61 % @Temperature 70.0 °C, Time 79200 sec |
61 % @Temperature 158 °F, Time 22.0 hour |
ASTM D395 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 227 °C | 441 °F | DSC |
| Glass Transition Temp, Tg | -15.0 °C | 5.00 °F | DSC |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 210 °C | 410 °F | Injection |
| Middle Barrel Temperature | 221 °C | 430 °F | Injection |
| Front Barrel Temperature | 229 °C | 444 °F | Injection |
| Nozzle Temperature | 232 °C | 450 °F | Injection |
| Melt Temperature | 232 °C | 450 °F | Injection |
| Drying Temperature | 104 °C | 219 °F | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
| Dew Point | -40.0 °C | -40.0 °F | |
| Hold Pressure | 5000 - 10000 MPa | 725000 - 1.45e+6 psi | Injection |
| Back Pressure | >= 50.0 MPa | >= 7250 psi | Injection |
| 10000 - 15000 MPa | 1.45e+6 - 2.18e+6 psi | Injection | |
| Screw Speed | 60 - 100 rpm | 60 - 100 rpm | Injection |