Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-FRG7.5 Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-FRHG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Drying Temperature | 82.2 - 121 °C | 180 - 250 °F | |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-GFMF2 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced Polybutylene Terephthalate, 40% Glass/Mineral ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-HG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy Polybutylene Terephthalate, 30% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Drying Temperature | 82.2 - 121 °C | 180 - 250 °F | |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Drying Temperature | 93.3 - 121 °C | 200 - 250 °F | Average value: 104 °C Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Drying Temperature | 80.0 - 121 °C | 176 - 250 °F | Average value: 109 °C Grade Count:6 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Drying Temperature | 75.0 - 121 °C | 167 - 250 °F | Average value: 111 °C Grade Count:22 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Drying Temperature | 116 - 121 °C | 241 - 250 °F | Average value: 121 °C Grade Count:19 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Drying Temperature | 121 - 121 °C | 250 - 250 °F | Average value: 121 °C Grade Count:8 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Drying Temperature | 121 - 121 °C | 250 - 250 °F | Average value: 121 °C Grade Count:9 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc. |