Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 100 - 110 °C | 212 - 230 °F | |
Polykemi AB POLYblend C65F PC/ABS-blend Information provided by Polykemi AB |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Drying Temperature | 80.0 - 110 °C | 176 - 230 °F | Average value: 101 °C Grade Count:14 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Requested for non-reinforced self-extinguishing types. Temperature can be reduced when using vacuum ovens. |
LATI LARIL 13 G/10 10% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Requested for non-reinforced self-extinguishing types. Temperature can be reduced when using vacuum ovens. |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | Average value: 107 °C Grade Count:5 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Drying Temperature | 100 - 110 °C @Time 14400 - 21600 sec |
212 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-601 UV PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Drying Temperature | 90.0 - 110 °C @Time 14400 - 21600 sec |
194 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PA66-R0N Flame Retardant PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelay, bobbins, plugsHousehold appliance partsE & E partsIn.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
LG Chemical LUCEL FW700S Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Drying Temperature | 90.0 - 110 °C @Time 14400 - 21600 sec |
194 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa CPA-6 Toughened PA6 Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 100 - 110 °C @Time 14400 - 21600 sec |
212 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa MAC-701 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Drying Temperature | 90.0 - 110 °C @Time 14400 - 21600 sec |
194 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose) Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Drying Temperature | 90.0 - 110 °C @Time 14400 - 21600 sec |
194 - 230 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Injection Molding |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Drying Temperature | 87.8 - 110 °C | 190 - 230 °F | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 104 - 110 °C | 220 - 230 °F | |
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 100 - 110 °C | 212 - 230 °F | Pre-drying |
Styrolution Luran® S KR 2861/1 C Colored ASA+PC Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh.. |