Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC30P105-08FA 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/30/E High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 238 °C | 400 - 460 °F | |
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 204 - 238 °C | 400 - 460 °F | |
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 204 °C | 399 °F | Injection |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 1020 GP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1020 GP is a 20% talc reinforced polypropylene homopolymer. It has applications in general purpose industrial, automotive, consumer, and construction.Data provided by Composite Technologies.. |
|||
Rear Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc.. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products CC30P100-00 30% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |