Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 2580 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 2510 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3500 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill and thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma .. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill an thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma r.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3601 General Purpose Crystal Polystyrene
(discontinued **) Easy flow for high productivity, excellent post molding scuff resistanceApplications: Medical, LabwareExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phys.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3700 General Purpose Crystal Polystyrene
(discontinued **) Good balance of flow and strength, Good crack resistanceApplications: Single service wares, Blending resinExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the .. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3930 General Purpose Crystal Polystyrene
(discontinued **) High melt flow, Crystal clearApplications: Razor components, Personal care, Thin wall moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and .. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 4211 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 4214 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5800 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |
|||
Mold Temperature | 49.0 - 82.0 °C | 120 - 180 °F | |
PolyOne Lubri-Tech™ AT-000/08T Acetal - 8% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 49.0 - 82.0 °C | 120 - 180 °F | |
PolyOne Lubri-Tech™ NL-40GB/15T Nylon 6/12 - 40% Glass Bead Reinforced - 15% PTFE Lubricated
(discontinued ** Data provided by PolyOne. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1504 High Heat Crystal Polystyrene Good balance of flow, strength and set up properties, Blue edge effect, USP Class VIApplications: Consumer electronics, Housewares, Cosmetic packagingExposure to gamma radiation in the 2.02-6.06 meg.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1510 High Heat Crystal Polystyrene High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
Mold Temperature | 66.0 - 82.0 °C | 151 - 180 °F | |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1220 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3511 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5124 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 4210 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5490 High Impact Polystyrene
(discontinued **) High heat, Good environmental stress crack resistance, Excellent printabilityApplications: Custom sheet, Lithographic applicationsProperties were determined on injection molded specimens at 23°C an.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5540 High Impact Polystyrene
(discontinued **) Excellent balance of toughness, flow, and set-up, High gloss, USP Class VIApplications: Structural foam, Housewares, Toys, Appliance parts, Dairy containersProperties were determined on injection mo.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 6100 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 2581 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistanceApplications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no significant eff.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 4501 Medium Impact Polystyrene
(discontinued **) Good toughnessApplications: Light louvers, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provide.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5504 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5530 High Impact Polystyrene
(discontinued **) Good overall balance of properties, Good toughnessApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |