| Category | Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded |
| Manufacturer | Polymer Technology & Services, LLC (PTS) |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PTS SAN-82TR SAN Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
| Melt Flow | 40 g/10 min @Load 10.0 kg, Temperature 220 °C |
40 g/10 min @Load 22.0 lb, Temperature 428 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 106 | 106 | ASTM D785 |
| Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
| Elongation at Break | 6.0 % | 6.0 % | ASTM D638 |
| Flexural Yield Strength | 113.1 MPa | 16400 psi | ASTM D790 |
| Flexural Modulus | 3.43 GPa | 497 ksi | ASTM D790 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 88.0 °C | 190 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 191 - 210 °C | 375 - 410 °F | |
| Middle Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
| Front Barrel Temperature | 216 - 229 °C | 420 - 445 °F | |
| Nozzle Temperature | 204 - 229 °C | 400 - 445 °F | |
| Mold Temperature | 48.9 - 79.4 °C | 120 - 175 °F | |
| Drying Temperature | 71.1 - 79.4 °C | 160 - 175 °F | |
| Dry Time | 2 - 3 hour | 2 - 3 hour | |
| Injection Pressure | 68.3 - 137 MPa | 9900 - 19800 psi | |
| Screw Speed | 40 - 100 rpm | 40 - 100 rpm |