| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized |
| Manufacturer | Ravago Manufacturing Americas, LLC |
| Trade Name | Hylon® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Ravago Manufacturing Americas Hylon® N2000NHL Nylon 6 (Cond).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | DAM; ASTM D792 |
| Water Absorption | 1.6 % | 1.6 % | 24 hrs, DAM; ASTM D570 |
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | 0.125 in, DAM; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
| Elongation at Break | 240 % | 240 % | ASTM D638 |
| Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
| Flexural Modulus | 0.945 GPa | 137 ksi | ASTM D790 |
| Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | 73°F; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | V-2 | V-2 | 0.0590 in, NC |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 238 - 266 °C | 460 - 510 °F | |
| Mold Temperature | 48.9 - 82.2 °C | 120 - 180 °F | |
| Drying Temperature | 73.9 °C | 165 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Moisture Content | 0.18 % | 0.18 % | |
| Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
| Screw Speed | 40 - 120 rpm | 40 - 120 rpm |