Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate Information provided by Ravago. |
|||
Mold Temperature | 26.7 - 93.3 °C | 80.0 - 200 °F | |
PTS Trimid® N66-SG33-BK 33% Glass Reinforced, High Impact Black Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 MK30HI 30% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Mold Temperature | 37.8 - 93.3 °C | 100 - 200 °F | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |