Polymer Property : Mold Temperature = 190 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized
High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced
Excellent Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Mold Temperature 71.1 - 87.8 °C
160 - 190 °F
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced
Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE
Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced
Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
Mold Temperature 71.1 - 87.8 °C
160 - 190 °F
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy
Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio..
Mold Temperature 71.1 - 87.8 °C
160 - 190 °F
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
Mold Temperature 71.1 - 87.8 °C
160 - 190 °F
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Mold Temperature 71.1 - 87.8 °C
160 - 190 °F
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Mold Temperature 71.1 - 87.8 °C
160 - 190 °F
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Mold Temperature 60.0 - 87.8 °C
140 - 190 °F
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond)
Information provided by Ravago.
Mold Temperature 60.0 - 87.8 °C
140 - 190 °F
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM)
Information provided by Ravago.
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
PolyOne Edgetek® XT XT-100-BU00 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
PolyOne Edgetek® XT XT-100-CX01 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
PolyOne Edgetek® XT XT-500-CX02 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Mold Temperature 48.9 - 87.8 °C
120 - 190 °F
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate
High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc.
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact
High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc.
Mold Temperature 60.0 - 87.8 °C
140 - 190 °F
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy
General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc.
Mold Temperature 48.9 - 87.8 °C
120 - 190 °F
Star Plastics PC/PBT7804 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
PolyOne Edgetek® XT XT-100-CX00 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
PolyOne Edgetek® XT XT-500-CX00 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..