Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
PolyOne Gravi-Tech™ GRV-UR-080-W Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Mold Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
Mold Temperature | 48.9 - 82.2 °C | 120 - 180 °F | |
Ravago Manufacturing Americas Hylon® N2000NHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Mold Temperature | 48.9 - 82.2 °C | 120 - 180 °F | |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3900 General Purpose Crystal Polystyrene
(discontinued **) High flow, Good compoundingApplications: Color concentrates, Compounding, Thin wall moldingsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and o.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 4211 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Mold Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Mold Temperature | 48.9 - 82.2 °C | 120 - 180 °F | |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Mold Temperature | 54.4 - 82.2 °C | 130 - 180 °F | |
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Mold Temperature | 48.9 - 82.2 °C | 120 - 180 °F | |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 3101 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Mold Temperature | 60.0 - 82.2 °C | 140 - 180 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Mold Temperature | 37.8 - 82.2 °C | 100 - 180 °F | |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Mold Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
Ecomass® 1003ZD95 Tungsten Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by.. |
|||
Mold Temperature | 57.2 - 82.2 °C | 135 - 180 °F | |
Ecomass® 1050ZD96 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and .. |
|||
Mold Temperature | 57.2 - 82.2 °C | 135 - 180 °F | |
Ecomass® 1700TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyRigidInformation provided by Technical Po.. |
|||
Mold Temperature | 57.2 - 82.2 °C | 135 - 180 °F | |
Ecomass® 1850ZD88 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Mold Temperature | 76.7 - 82.2 °C | 170 - 180 °F | Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products. |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 37.8 - 82.2 °C | 100 - 180 °F | Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products. |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 37.8 - 82.2 °C | 100 - 180 °F | Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products. |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5420 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5490 High Impact Polystyrene
(discontinued **) High heat, Good environmental stress crack resistance, Excellent printabilityApplications: Custom sheet, Lithographic applicationsProperties were determined on injection molded specimens at 23°C an.. |
|||
Mold Temperature | 38.0 - 82.0 °C | 100 - 180 °F | |
Ineos Nova 5711 High Impact Polystyrene
(discontinued **) High flow, High impact, USP Class VIApplications: Thin wall, Medical, Housewares, ToysProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Inform.. |