Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristics: High Str.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TP-HG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy Polybutylene Terephthalate, 30% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Mold Temperature | 60.0 - 87.8 °C | 140 - 190 °F | |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BU01-HF Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 48.9 - 87.8 °C | 120 - 190 °F | |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
Mold Temperature | 48.9 - 87.8 °C | 120 - 190 °F | |
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled 30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded 13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Mold Temperature | 65.6 - 87.8 °C | 150 - 190 °F | |
PolyOne Edgetek® XT XT-500-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |