Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 60.0 - 71.1 °C | 140 - 160 °F | |
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Mold Temperature | 60.0 - 71.1 °C | 140 - 160 °F | |
PolyOne Trilliant™ HC HC6620-0033 RS Natural Polyamide 66 (Nylon 66) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Mold Temperature | 48.9 - 71.1 °C | 120 - 160 °F | |
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 21.1 - 71.1 °C | 70.0 - 160 °F | |
Northstar Polymers MPA-A30B Mold-Making Resin MPA-A30B is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | Cavity mold surface temperature at equilibrium conditions |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | Cavity mold surface temperature at equilibrium conditions |
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components |
|||
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | |
PTS Trilac® ABS-EX1000 High Impact Extrusion Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 48.9 - 71.1 °C | 120 - 160 °F | |
PolyOne Lubri-Tech™ SY-000/10T-2S Natural Polystyrene (PS), PTFE Lubricated
(discontinued **) Description/Features:High ImpactPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 65.6 - 71.1 °C | 150 - 160 °F | |
PolyOne Edgetek® ATH-10CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 60.0 - 71.1 °C | 140 - 160 °F | |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 40.6 - 71.1 °C | 105 - 160 °F | |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 10.0 - 71.1 °C | 50.0 - 160 °F | |
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 54.4 - 71.1 °C | 130 - 160 °F | |
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 10.0 - 71.1 °C | 50.0 - 160 °F | |
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc. |