Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom PLASTALEN® PH 91 SDU Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o. |
|||
Mold Temperature | 40.0 - 50.0 °C | 104 - 122 °F | |
Plastcom SLOVALEN PC 53 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PC 71 GF 10 PP, 10% glass fibre FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass fibre and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F | |
PolyOne Maxxam™ DP-9162-3 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F | |
PolyOne Maxxam™ NT-818.G002-8000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F | |
PolyOne Maxxam™ PPC-40C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Mold Temperature | 16.0 - 50.0 °C | 60.8 - 122 °F | |
PolyOne Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
Inno-Comp INNOPOL® CS 2-3840 MO 40% Glass Filled Polypropylene Copolymer INNOPOL® CS 2-3840 MO is a 40 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-3840 MO is recommended for p.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Solvay TECHNYL® C 216 PA6, DRY Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | Injection Molding |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ EG203AE Polypropylene Compound Elastomer and Mineral Modified Daplen EG203AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EG203AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai.. |
|||
Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | EBM Blow Mold Temp. |
Eastman Tritan WX500 Copolyester Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Eurostar Starflam MF0044 PP, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam MF0044 is a Halogen Free Flame Retardant, Glass Fiber Reinforced, PP Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Eurotec® Tecolen® CP10 GR15 NL PPCP, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Eurotec® Tecolen® CP10 GR30 NL PPCP, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Eurotec® Tecolen® CP20 GB30 NL PPCP, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Mold Temperature | 10.0 - 50.0 °C | 50.0 - 122 °F | Injection |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Plastcom SLOVALEN PQ 53 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |
|||
Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
Polykemi AB POLYfill PPH DNH15025 GF10 Polypropylene Homopolymer, Flame Retardant, Halogen Free, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
Borealis Daplen™ KB4436 TPO Compound Daplen KB4436 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen KB4436 is a material with excellent impact/stiffness ratio. Thanks to its low the.. |
|||
Mold Temperature | 25.0 - 50.0 °C | 77.0 - 122 °F | |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |