Material Notes:
FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
Linear Mold Shrinkage 0.0252 cm/cm
0.0252 in/in
Linear Mold Shrinkage, Transverse 0.0263 cm/cm
0.0263 in/in
Melt Flow 11 g/10 min

@Load 0.325 kg,
Temperature 270 °C
11 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
Elongation at Break 7.5 %
7.5 %
Tensile Modulus 0.840 GPa
122 ksi
Flexural Strength 22.0 MPa
3190 psi
Flexural Modulus 0.750 GPa
109 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
Charpy Impact, Notched 4.40 J/cm²

@Temperature -20.0 °C
20.9 ft-lb/in²

@Temperature -4.00 °F
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 140 °C
284 °F
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Vicat Softening Point 95.0 °C
203 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Pressure 60.0 - 70.0 MPa
8700 - 10200 psi