Polymer Property : Mold Temperature = 150 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 80.0 - 150 °C
176 - 302 °F
PolyOne Edgetek® QT-20MN/000 natural HI Syndiotactic Polystyrene (SPS)
Information provided by PolyOne
Mold Temperature 100 - 150 °C
212 - 302 °F
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Mold Temperature 100 - 150 °C
212 - 302 °F
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber
Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non..
Mold Temperature 110 - 150 °C
230 - 302 °F
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Mold Temperature 130 - 150 °C
266 - 302 °F
Injection Molding
LG Chemical LUCON CP510F PC/ABS+CNT
Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b..
Mold Temperature 130 - 150 °C
266 - 302 °F
Injection Molding
LG Chemical LUCON PN9009 PPS+MF
Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2..
Mold Temperature 80.0 - 150 °C
176 - 302 °F
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Mold Temperature 80.0 - 150 °C
176 - 302 °F
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Mold Temperature 80.0 - 150 °C
176 - 302 °F
Injection Molding
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose
Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical
Mold Temperature 80.0 - 150 °C
176 - 302 °F
Injection Molding
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant
Feature: Injection Molding, sPS+GF30%, Flame RetardantApplication: Pump Units, Pick-up Lends Holder, etcCAS No. 9003-53-6, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical
Mold Temperature 130 - 150 °C
266 - 302 °F
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Mold Temperature 130 - 150 °C
266 - 302 °F
LATI Latilub 80-10T K/15 PPS, 15% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Mold Temperature 130 - 150 °C
266 - 302 °F
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Mold Temperature 130 - 150 °C
266 - 302 °F
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Mold Temperature 130 - 150 °C
266 - 302 °F
Covestro Apec® 2095 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content
Mold Temperature 130 - 150 °C
266 - 302 °F
Eurostar Starflam UF0033 PPA, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam UF0033 is a Mineral Flame Retardant, Halogen Free and Red Phosphorous Free, Glass Reinforced, Polyphthalamide Injection Molding ResinInformation provided by Eurostar.
Mold Temperature 135 - 150 °C
275 - 302 °F
Beijing Chemical Industry KAIFA® S-114 PPS Resin
Glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group)
Mold Temperature 100 - 150 °C
212 - 302 °F
LATI LAESTRA G/40-V0CT1 40% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Mold Temperature 40.0 - 150 °C
104 - 302 °F
E-Polymers SEPAZ® C140GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Mold Temperature 40.0 - 150 °C
104 - 302 °F
E-Polymers SEPAZ® C240GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Mold Temperature 100 - 150 °C
212 - 302 °F
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)  (discontinued **)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..