Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-7315 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-7854 PBT, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-7952 PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-8023 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-8282 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Nozzle Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® SG5300 PBT+PET+GF30% Description: Injection Molding, PBT+PET+GF30%, Good Surface Application: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5100 PC/ABS+GF10% Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | |
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 265 °C | 500 - 509 °F | |
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 260 - 265 °C | 500 - 509 °F | |
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |