Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Honeywell Aegis™ PL56HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL56HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt v.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 240°C |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR474 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 260 °C | 446 - 500 °F | |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 230 °C | 446 °F | C5 |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 235 °C | 446 - 455 °F | |
Solvay TECHNYL® C 246 M PA6, DRY Description: Unreinforced polyamide 6, with high impact resistance, for injection molding. Grade formerly known as PSB196.Available in: EuropeProduct Applications: It is particularly adapted to the .. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Front Barrel Temperature | 230 °C | 446 °F | |
Solvay TECHNYL® C 507XT PA6, DRY Description: Unreinforced polyamide 6, heat stabilized, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rod.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 280 °C | 446 - 536 °F | |
Teknor Apex Beetle® MDF50 Nylon 6, 50% Short Glass Fiber Filler Notes: MDF50 is a 50% glass fiber reinforced nylon 6 that offers excellent mechanical performance coupled with good surface finish Features: Good Surface FinishProcessing Method: Injection molding F.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Unitika A3130 PA6, 35% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | >= 230 °C | >= 446 °F | |
Borealis Daploy™ SF203HMS High Melt Strength Polypropylene for Extrusion Coating Daploy SF203HMS resin is a statistic-heterophasic-propylene-ethylene copolymer modified with a polypropylene based structurally isomeric polymer which combines a significantly increased melt strengt.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR404T ABS, Heat Resistance Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical.. |